Elcometer 106/6 混凝土涂层附着力测试仪

Elcometer 106/6 附着力测试仪特别为测试混凝土上的涂层而设计。

Elcometer 106/6与 Elcometer 106 附着力测试仪操作方法类似,使用的是50mm (2”) 直径的锻模,测试混凝土上的涂层。

Elcometer 106/6是完全便携的,并供应在一个手提箱-使其成为理想的现场测试。

Elcometer 106/6 混凝土涂层附着力测试仪
Elcometer 106/6 混凝土涂层附着力测试仪Elcometer 106/6 混凝土涂层附着力测试仪Elcometer 106/6 混凝土涂层附着力测试仪

附件

部件编号 产品描述 证书
F106----6 Elcometer 106 混凝土涂层附着力测试仪——范围 6 ο
范围 0 - 3.5MPa (N/mm2) 0 - 500psi  
尺寸 505 x 370 x 120mm (19.9 x 14.6 x 4.7")  
套装毛重 5.7kg (12.6lb)  
包装清单 Elcometer 106/6混凝土涂层附着力测试仪主机, 5 x 50mm (2”) 锻模, 支撑环, Araldite 胶, 棘轮扳手, 手提箱和操作手册 

 

遵从如下标准:
ASTM D 7234, BS 1881-207, DIN 1048-2, EN 1542, EN 12636

ο 可选择提供校准证书。

技术规格

T10618570 备用锻模,直径50mm (2”) (5个装)
T99912906

Araldite标准两部分环氧粘合剂,2 x 15ml软管

KT001910P122 切割工具,用于 50mm (2”) 直径的锻模

视频

1. An Introduction to Pull-Off Adhesion on Coated Surfaces

Adhesion testers are used to test how well a coating has adhered to a surface, as poor adhesion can lead to premature coating failures. The coating inspector has essentially three main methods to choose from - cross hatch, push off, and the most common, the pull-off adhesion test.

 

This video is part of a series on Pull-Off Adhesion Testing, to see the next video please click here.

To download the video script in English click here.

相关视频

1. An Introduction to Pull-Off Adhesion on Coated Surfaces
1. An Introduction to Pull-Off Adhesion on Coated Surfaces

Adhesion testers are used to test how well a coating has adhered to a surface, as poor adhesion can lead to premature coating failures. The coating inspector has essentially three main methods to choose from - cross hatch, push off, and the most common, the pull-off adhesion test.

 

This video is part of a series on Pull-Off Adhesion Testing, to see the next video please click here.

To download the video script in English click here.

//www.youtube.com/embed/pHvgjZZ3cRg
2. Selecting the Dolly Diameter and Gauge
2. Selecting the Dolly Diameter and Gauge

When it comes to selecting the dolly diameter and adhesion gauge type to use for a pull-off adhesion test; factors such as the substrate material, the substrate shape, and the expected coating strength will affect the dolly or gauge the user chooses.

 

This video is part of a series on Pull-Off Adhesion Testing, to see the next video please click here.

To download the video script in English click here.

//www.youtube.com/embed/NQdcl-EyEJU
3. Selecting the most Appropriate Position for an Adhesion Test
3. Selecting the most Appropriate Position for an Adhesion Test

When preparing a pull-off adhesion test, whilst the actual location and the number of pulls is typically defined by the test method or procedure that’s being followed, the actual positioning of the dolly is vital, as poor positions can result in low pull-off values or invalid tests.


 

This video is part of a series on Pull-Off Adhesion Testing, to see the next video please click here. 

To download the video script in English click here.

 

//www.youtube.com/embed/s30uCK_U44w
4. Preparing the Dolly and the Coating
4. Preparing the Dolly and the Coating

Properly preparing the dolly and the surface before performing a pull-off adhesion test will help achieve higher pull-off values.

 

This video is part of a series on Pull-Off Adhesion Testing, to see the next video please click here.

To download the video script in English click here.

 

//www.youtube.com/embed/UJYYe_NZ9YQ
5. To Cut or Not to Cut?
5. To Cut or Not to Cut?

Should the coating around a dolly be cut, or left uncut prior to a pull-off adhesion test; and whose decision is it to make?

 

This video is part of a series on Pull-Off Adhesion Testing, to see the next video please click here.

To download the video script in English click here.

//www.youtube.com/embed/avSFGkyVAd8
6. The Pull-Off Test
6. The Pull-Off Test

Once the glue between a properly prepared dolly or pull stub and a properly prepared coating has fully cured, the pull-off adhesion test can be undertaken using the adhesion tester of choice.

 

This video is part of a series on Pull-Off Adhesion Testing, to see the next video please click here.

To download the video script in English click here.

 

//www.youtube.com/embed/uJXt0Pbrj0k
7. Assessing the Result; Glue, Adhesive and Cohesive Failures
7. Assessing the Result; Glue, Adhesive and Cohesive Failures

Once the pull-off adhesion test has been completed the tensile pull-off force, whether the coating was coat or not, the dolly size and gauge type, and the failure mode of the coating are all recorded; with the nature of the failure usually recorded as an estimated percentage to the nearest 10%.

 

This video is part of a series on Pull-Off Adhension Testing, to view the playlist please click here.


To download the video script in English click here.

//www.youtube.com/embed/2OG23w7Ww9Q
<P> 8. Measuring the Pull-Off Adhesion of Coatings on Concrete</P>

 8. Measuring the Pull-Off Adhesion of Coatings on Concrete

Testing coating adhesion on concrete substrates using a pull-off adhesion gauge is similar to testing coatings on metal substrates. However, there are a number of differences in the test procedures and equipment used.


This video is part of a series on Pull-Off Adhension Testing, to view the series playlist please click here.


To download the video in script in English click here.

//www.youtube.com/embed/CoURXuYVnAg